X2CrNiMo17 12 2 14404 SteelNumber Chemical

X2CrNiMo17 12 2 / 1.4404 SteelNumber Chemical

X2CrNiMo17 12 2 (1.4404) Chemical composition % of steel X2CrNiMo17 12 2 (1.4404)EN 10088 2 2005 Particular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted.DIN EN 1.4404 Material X2CrNiMo17 12 2 Stainless Steel EN 1.4404 Stainless Steel (X2CrNiMo17 12 2) EN 1.4404 material (stainless steel X2CrNiMo17 12 2) is a low carbon version of 1.4401 (X5CrNiMo17 12 2), the maximum carbon content is only 0.03%, while 1.4401 is 0.07% maximum, so the weldability and corrosion resistance of 1.4404 stainless steel 316L ( AISI, ASTM, UNS) Worldwide Steel NumberChemical composition and properties of european equivalents (EN) for 316L (USA, AISI, ASTM, UNS)X2CrNiMo17 12 2 (1.4404) , X2CrNiMo17 12 3 (1.4432) , X2CrNiMo18 14 3 (1.4435) , 316L (USA, AISI, ASTM, UNS ) European (EU, EN) and wordwide Steel equivalent grades These comparison table is only intended as an indication of the closest khown

X2CrNiMo17 12 (UNI ) Worldwide equivalent grades

X2CrNiMo17 12 2 (1.4404) , X2CrNiMo17 12 (Italy, UNI ) European (EU, EN) and wordwide Steel equivalent grades These comparison table is only intended as an indication of the closest khown equivalent grades. The source standarts should always be checked for the specific purpose for each material, in case of doubt Buy, sell, suppliers search 1.4404 (AISI 316 L), S31603 Datasheet METALCORDescription 1.4404 / AISI 316 L is an austenitic chromium nickel molybdenum stainless steel with low carbon content.Stainless Steel 316, 1.4401, UNS31600, X2CrNiMo17 12 2 stainless steel coil and plate 316, 1.4401, UNS31600, X2CrNiMo17 12 2, Coil and Plate. We stocks and supplies only dual certified 316 grade sheet certified.

X2CrNiMo17 13 2 (DIN, WNr ) Worldwide equivalent grades

X2CrNiMo17 12 2 (1.4404) , X2CrNiMo17 13 2 (Germany, DIN, WNr ) European (EU, EN) and wordwide Steel equivalent grades These comparison table is only intended as an indication of the closest khown equivalent grades. The source standarts should always be checked for the specific purpose for each material, in case of doubt Buy, sell, suppliers Z2CND17 12 (AFNOR NFA ) Worldwide equivalent gradesfor Steel Z2CND17 12 (AFNOR NFA) and its European equivalent X2CrNiMo17 12 2 (1.4404) (EN) European equivalent grade for Austenitic stainless steel Z2CND17 12 (AFNOR NFA)X2CrNiMo17 12 2 (1.4404) NEW opportunities for buyers! Post free buying requirement for product Z2CND17 12 AISI 316, AISI 316L, 1.4404, 1.4401 stainless steel1.4404, 1.4401, AISI 316/L application and specification. Austenitic stainless steel is resistant to intergranular corrosion, used mainly in environments containing harmful chlorides, acids and urea. 316/316L is the basic grade from the CrNiMo group with Molybdenum, the addition of which significantly increases the resistance to pitting and crevice corrosion of steel by 2 3 times.

DIN EN 1.4401 Material X5CrNiMo17 12 2 Stainless Steel

Due to the chemical composition of molybdenum, its corrosion resistance is higher than 1.4301 (X5CrNi18 10), especially in environments containing chloride and non oxidizing acids. 1.4404 (X2CrNiMo17 12 2) is an ultra low carbon version of 1.4401 stainless steel, which has better corrosion resistance in welded structures.X2CrNiMo17 12 2 1.4404) 316L Z3CND18 316S11 Equivalent References Germany, DIN X2CrNiMo17 12 2 Japan, JIS SUS316L France, AFNOR Z12CMN17 07Az USA,  316L Detailed Feature Table1.4404 x2crnimo17 from stock Data Sheet1.4404 is a low carbon, austenitic chromium nickel molybdenum steel. Due to the addition of 2 2.5% molybdenum, the corrosion resistance of the 1.4404 is significantly better than that of the standard austenitic grades 1.4301 and 1.4307.. The material 1.4404 is resistant to intercrystalline corrosion when welded! but not resistant to sea water.

SAINLESS SEELS 316L 316LUS RODACCIAI SPA

X2CrNiMo17 12 2 1.4404 X 2 CrNiMo 17 12 X2CrNiMo17 12 2 1.4404 Z3 CND 17 11 02 (316S11) 316L MECHANICAL PROPERTIES Cold drawn (2H, 2B) and ground bars (2G) in the solution annealed condition Size max (mm) Rp1.4404 /DIN X2CrNiMo17 12 2 datasheet,1.4404 /DIN 1.4404 /DIN X2CrNiMo17 12 2 2014 11 24 10:04:33 Origin Remark 0 Click Technical specifications of X2CrNiMo17 12 2 austenitic stainless steel Chemical composition, mechanical properties from steelmaking,forging,rolling,heat treatment,cold working.We also possess advanced precision machining equipments for further processingX2CrNiMo17 12 2 steelThis page cover the X2CrNiMo17 12 2 chemical element, Mechanical Properties, X2CrNiMo17 12 2 Datasheet, Cross Reference of X2CrNiMo17 12 2 steel, Mainly used for .

1.4404 woite edelstahl

EN symbol (short) X2CrNiMo17 12 2AISIAISI 316 L UNSS 31603 Grade TP 316 LAFNORX2CrNiMo17 12 2 / NF EN 10028 7 (01/2000) (FR) BSX2CrNiMo17 12 2 / B.S.EN 10028 7 (01 2000 ) Stainless Steel EN 1.4404 AISI 316L X2CrNiMo17 12 2 UNS Reliable Steel is one of the leading manufacturers, exporters, stockiest, distributors, dealers and suppliers of superior quality Stainless Steel & High Nickel Alloys Pipes, Tubes, Plates, Sheets, Round Bars, Fittings & Forgings in different specifications, which find application in high demanding industries and sectors, particularly high temperature and corrosive services.X2CrNiMo17 13 2 (DIN, WNr ) Worldwide equivalent gradesX2CrNiMo17 12 2 (1.4404) , X2CrNiMo17 13 2 (Germany, DIN, WNr ) European (EU, EN) and wordwide Steel equivalent grades These comparison table is only intended as an indication of the closest khown equivalent grades. The source standarts should always be checked for the specific purpose for each material, in case of doubt Buy, sell, suppliers

EN 1.4404 / AISI 316L *AISI 316L

EN 1.4404 / AISI 316L *AISI 316L. Euronorm Nom. AISI / ASTM / UNS; 1.4404X2CrNiMo17 12 2316L / * 316LChemical composition. Grades C Si Mn P S Cr Ni Mo Ti Cu Other; ACX 240 =0.030 =0.75 =2.00 =0.040 =0.03016.00 18.0010.00 12.002.00 2.50 ACX 332 =0.030AISI 316, AISI 316L, 1.4404, 1.4401 stainless steel1.4404, 1.4401, AISI 316/L application and specification. Austenitic stainless steel is resistant to intergranular corrosion, used mainly in environments containing harmful chlorides, acids and urea. 316/316L is the basic grade from the CrNiMo group with Molybdenum, the addition of which significantly increases the resistance to pitting and crevice corrosion of steel by 2 3 times.Material Data Sheet 1.4404, 316L, S 31603 :M. Woite GmbHX2CrNiMo17 12 2 X 2 CrNiMo 17 13 2AISI/SAE316LUNS Standards Description. The austenitic stainless steel 1.4404 (316L) shows good acid resistance. Material 1.4404 (316L) is used in the chemical industry, apparatus engineering, sewage plants, and paper industry. Our product range in 1.4404 (316L) are tubes and pipes, fittings and

Steelinox Stainless Steel AISI 316L / 1.4404 Steelinox

Translate this page1.4404 / AISI 316L / X2CrNiMo17 12 2. We do this for various customers in the machining industry, mechanical engineering, (petro) chemical, offshore and aerospace industries. Steelinox is the right partner if your material requirements are high. Contact Call us at +31 (0)186 651 004EN 10216 5 X2CrNiMo17 12 2 Stainless Steel Pipes & Tube What is EN 10216 5 X2CrNiMo17 12 2? Chemical Composition & Mechanical Properties of EN 10216 5 X2CrNiMo17 12 2. Specifications for EN 10216 5 X2CrNiMo17 12 2 Steel PipesAbout DIN 17456 "X2CrNiMo17 12 2" Chemical, DIN 17456 General Purpose Seamless Circular Stainless Steel Tubes Specification DIN 17456 General Purpose Seamless Circular Stainless Steel Tubes Standard DIN 17456 Equivalents DIN 17458, GOST 9941 81, GOST 9940 81, ASME SA213, ASTM A213, EN 10216 5 Materials X2CrNiMo17 12 2, 1.4404 Chemistry Composition of DIN 17456 X2CrNiMo17 12 2, 1.4404 C, % Si, % Mn, % P,

Get In Touch With